easley59 on wed 24 mar 04
Look in the archives, subject "underglaze pencils".
I generally read my List via eScribe, and it's easy getting to a thread =
index from there, too.
This was discussed quite some time ago and there are a number or recipes =
for you there.
I never did make any, but sounds like fun.
Let us know how you do........
Pam in Seattle
Ron Collins on fri 26 mar 04
Last year, I posted a recipe for "roll your own" underglaze pencils, that
cost practically nothing......they work fine..........Melinda Collins,
Antigua, Guatemala
Lee Love on sat 27 mar 04
Ron Collins wrote:
>Last year, I posted a recipe for "roll your own" underglaze pencils, that
>cost practically nothing......they work fine..........Melinda Collins,
>Antigua, Guatemala
>
>
>
Melinda, I found this in the archives:
>>I just used equal parts ball clay, talc, and added colorants/oxides to
>>taste, and rolled my own....can sharpen with little pencil sharpener...they
>>work fine.....I fired to about 800 c. Melinda
>
--Lee In Mashiko Lee@Mashiko.org http://Mashiko.us
"With Humans it's what's here (he points to his heart) that makes
the difference. If you don't have it in the heart, nothing you make will
make a difference." ~~Bernard Leach~~ (As told to Dean Schwarz)
| |
|