Hey Folks.
In the past I have used a product called OPC8 covercoat to paint over
decals done by laser printer. When I used this product all the images
came out sharp and didnt smear, and it didn't have a strong solvent
odour. I have recently tried Decal magic and and a new batch of the
OPC8, and have found that both of them smell solvent like, and destroy
the image done by the laser printer. Would anyone know a source for the
old OpC8 or know of a product that could work for this process.