IV-14 Oxidation Copper Reduction
(cone 9-10)

Kona F-4 spar 6.88%
Silica 25.78%
Calcined borax 2.06%
Whiting 13.73%
Tin oxide 1.04%
Copper Carbonate .29%
Silicon carbide (FFF grain) .31%
SS-65 brand sodium silicate 1.24%
ferro frit 3191 .31%
EPK 1.38%
Zinc oxide 2.60%
ferro frit 3134 5.48%
Kona A-3 spar 38.90%

Most things are still available, what can sub for those that are not?