search  current discussion  categories  glazes - misc 

low temp glaze

updated wed 7 apr 04

 

paulo velho on tue 6 apr 04


Hi,

I'm looking for a recipe of a very low temperature glaze (around cone 020)
that can be used with very bright colorants (strong blue and yellow, for
instance). The idea is to use it in termites nest for an installation about
ceramic making process. I would appreciate if someone has a formula.

regards

paulo velho

Ababi Sharon on tue 6 apr 04


Hello
paulo velho
Try to use a low alumina sodium frit as it is.

Ababi Sharon
Glaze wizard
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
A fast link Ceramics forum in Hebrew:
http://www.botzpottery.co.il/kishurim.html

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of paulo velho
Sent: Tuesday, April 06, 2004 5:08 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: low temp glaze

Hi,

I'm looking for a recipe of a very low temperature glaze (around cone
020)
that can be used with very bright colorants (strong blue and yellow, for
instance). The idea is to use it in termites nest for an installation
about
ceramic making process. I would appreciate if someone has a formula.

regards

paulo velho

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.