Randy McCall on sat 10 apr 04


I had previously tested this glaze with a thin coat and I got a golden =
varigated matt glaze that broke to a tanish white.

I tried it on a number of pieces but put two rather thick coats on and =
got a runny ash type glaze, but it had bubbles in the rivilets that were =
thick. =20

I also fired at cone 7 instead of cone 6.

Is there anyway to refire and save these pieces or am I wasting my time =
and effort. Anything I can do?