Betsy Price/Tom Wirt on fri 9 apr 04
Some ilmenite seems to have changed. We're looking for anyone who might
have a few pounds of Milled (or Powdered) Ilmenite from MileHi Ceramics in
Denver from a year or two ago that they'd be willing to sell.
We think the issue is with the mesh of the grind and are testing samples
from various suppliers and finding a wide variety in the results.
Thanks in advance. You can answer directly to claypot@hutchtel.net