A glaze formula calls for Frit 3626. Is there another equivalent to this one?

Llewellyn Kouba
Abbey Pottery

Ababi Sharon on mon 12 apr 04


From Tony Hansen:
FRIT 3626
Description: LEAD BISILICATE
Date: 09/05/97
Supplier: FERRO
Melts At: 820C M
SpecGravity: 4.50
Family: 5-Frit
FRIT 3626 Notes
A 65% PbO well tied up lead source.

Ababi

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Llewellyn
Kouba
Sent: Monday, April 12, 2004 6:21 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Help on frit 3626

A glaze formula calls for Frit 3626. Is there another equivalent to this
one?

Llewellyn Kouba
Abbey Pottery

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.