raku pot rims

updated wed 14 apr 04

 

COREY J SCHMIDT on mon 12 apr 04


I didn't throw as many pot as I had wanted. But I must say, using the
plastic bag to finish the rims on the heavily grogged Raku pots seems to be
just the trick! Thanks for the simple, but oh so effective remedy for my
problem!