search  current discussion  categories  forms - handles 

putting on cane handle

updated thu 15 apr 04

 

MarjB on wed 14 apr 04


Afternoon: If the handle is too big for your pot - soak it as =
suggested, with the rings on the tails, then bend it gently to the size =
you need. Next, wire/string the handle to hold that size. A little over =
sized is better than undersized. Leave it wired to size for a day or =
two. You may have to weight it with bricks or something similar so that =
it doesn't twist out of shape as it is drying.=20
Then resoak to soften tails to fit into lugs. Suggest you put spout =
side in first.
Wish you success. Enjoy your tea. MarjB