Sajans Raku , similar to copper sand but glossy surface.
Colors range from rich hunter dreens without reduction to
various coppers, golds, greens and reds when reduced.
I have found it applies very well.
gerstly borate 72.5
soda feldspar 18.12
copper cardonate 8.9
Angela Davis
"Have joy in everything you make."
Had a wonderful time at class tonight, my Henko bottle was out of
the kiln and looks pretty darn good, we did some horsehair and I
got the nicest one since I started a year ago. I'll try to get pictures =
up
tomorrow.
| |
|