search  current discussion  categories  glazes - crazing & crackle 

non craze glaze/food safe

updated fri 30 apr 04

 

MarjB on fri 30 apr 04


Morning Joseph

If you have not tried/tested the basic cone 10 glazes on digitalfire.com =
I would suggest that as a good start. Have you checked the absorption =
of your claybody lately ? Might be a combination of solutions. MarjB