search  current discussion  categories  glazes - specific colors 

mayco stroke and coat on green ware?

updated fri 7 may 04

 

Julie Beutler on thu 6 may 04


Once we had a small amount of it put on a green ware piece and it was =
fine, we just took it to bisque and then applied clear and to bisque =
temp again, but you know different clay body and all plus it was only a =
little area...I was more curious that you wrote Cone 5....I think that =
stroke and coat is low fire....but maybe we are talking about 2 =
different things or maybe you push yours to a different temperature. =
I'd be interested in hearing if you have had success taking it to cone 5 =
though!

hope this helps-
Julie Beutler