Richard Mahaffey on sat 19 jun 04
Hello Clayarters,
I forgot one critical step in the process for making the celadon using
the base glaze that I posted last night. You should ball mill or
otherwise grind the Red Iron Oxide to avoid the dreaded iron spots.
Rick
| |
|