=?iso-8859-1?q?Marilu=20Tejero?= on tue 13 jul 04
Anyone experimenting with Michael Bailey's alumina semimatts and matts please contact me in private.
Getting some good buttery smooth surfaces and others extremely dry.
Also, I need to advise on a firing cicle for ^ 6 on a Skutt kiln.. I don't want to rely on a cone sitter and need to know how long does it take to complete it. I would need to be present at the end of the firing and live 16 miles away from where the studio is.
Depending the hour, this means, 30 minutes or one hour and a half.
Thanks