Ron Roy on tue 27 jul 04
Alumina has no significant hazards for the potter - you should not breath
the dust but it is not absorbed through the skin from the hydrate or
calcined material.
RR
>from what I've heard, alumina can be absorbed through the skin, so handling
>raw
>alumina hydrate or oxide may be risky.
>
Ron Roy