This combo, cobalt carb + black iron oxide circa 4:1, plus china clay =
and some glaze slop, is what I use for drawing on delft type tiles. Very =
dark navy blue, excellent for a clean line. I got it from a book on =
tiles by a man named Jones. Mel, your schlock is my standby.