John Hesselberth on wed 18 aug 04
firing schedules?
On Tuesday, August 17, 2004, at 10:05 PM, June Perry wrote:
> About a month or two ago someone posted a link showing pictures of
> some cone
> 6 glazes and the difference in color between those fired just to cone
> 6 and
> those fired cone 6 with a firing down schedule.
> I mentioned this to a friend who has some people at her studio working
> in
> cone 6 and told her I'd try to get the link but I haven't been able to
> find it in
> searching the archives all the way back to June.
> I'd appreciate if the person who posted the original link or anyone
> else who
> might have saved it to please email me with the information.
Hi June,
You can see one set of photos at
http://www.masteringglazes.com/Pages/faqframe.html
Read question 2 and then click on 'Click here'. Also a significant part
of my last NCECA presentation was devoted to that subject. The
presentation starts at
http://www.frogpondpottery.com/nceca2004/p01.html
but the photos of fast, slow and very slow cooling start at
http://www.frogpondpottery.com/nceca2004/p18.html
Regards,
John
John Hesselberth
http://www.frogpondpottery.com
http://www.masteringglazes.com
| |
|