Hello Everyone,

I have heard so many good things about ITC. I have decided to try it. I use
a cone 10 porcelain. It has been suggested after coating the shelves with
ITC 100, I should apply some ITC 296-A for extra purity in my porcelain firings.
I have not heard anyone talk about this product. I just bought some new
Acme Marls High Alumina shelves. I don't want to ruin them. Any information
would be appreciated.

Thanks,

Teresa Testa,
Windancer Studio
Las Vegas, Nevada

Ian Walruth on wed 1 sep 04


The ITC 296 is (according to Nils Lou) supposed to harden the ITC 200 and
seal it.

>Teresa wrote:
>
> I have heard so many good things about ITC. I have decided to try it. I use
> a cone 10 porcelain. It has been suggested after coating the shelves with
> ITC 100, I should apply some ITC 296-A for extra purity in my porcelain
> firings.
> I have not heard anyone talk about this product. I just bought some new
> Acme Marls High Alumina shelves. I don't want to ruin them. Any information
> would be appreciated.
>
>