Brian Haviland on tue 14 sep 04
At 03:28 PM 9/13/04 -0500, you wrote:
>.
>
>When I throw largish bowls or platters, I often lose them to
>cracking. Sometimes the crack shows after the bisque firing and sometimes
>after the glaze firing. Sometimes it is a smallish "s" type crack, but
>often it is larger & all the way through the piece.
>
>
>Hello sue
Look in the archives under s-cracks and you will find
more info than you can imagine..My guess is you need to
compress the bottoms more..but that's just my 2 cents..
> Brian
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.
Brian Haviland
Fountain city, Indiana
Haviland Stone Pottery & Raku
bnhavil@greentokai.com
"Accept the things to which fate binds you, and love the people with whom
fate brings you together, but do so with all your heart."
Notice: "If you are not the intended recipient of this E-mail, be aware that any disclosure, copying, distribution, or use of this e-mail and/or any attachments is prohibited. If you have received this e-mail in error, please notify the sender immediately and delete this copy and any attachments hereto from your system. Thank you for your anticipated cooperation."
| |
|