: making glaze

updated tue 21 sep 04

 

Lee Love on tue 21 sep 04


Scaleless mixing:

last batch Nami Jiro:


50 ladles wood stove ash slurry
30 ladles gariomi ball clay slip
10 ladles Amakusa (porcelain stone.) slip


--
Lee in Mashiko, Japan http://mashiko.org