xavier warm jade question

updated sat 2 oct 04

 

Daraburn@AOL.COM on tue 28 sep 04


I have used this glaze (from CM) periodically with no problems but I just
fired a mug with XWJ on the inside and 1/3 down on the outside. The bottom 2/3
outside of the mug is MC6G Clear Liner. The XWJ crazed on the inside! If
anyone is familiar with this glaze can you tell me what happened and how to fix
it?

Dawn in Tennessee

Donna Nicosia on tue 28 sep 04


Sounds like a nice color glaze. Do you know what issue cm it is in?
Donna

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of
Daraburn@AOL.COM
Sent: Tuesday, September 28, 2004 8:12 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Xavier Warm Jade question

I have used this glaze (from CM) periodically with no problems but I
just
fired a mug with XWJ on the inside and 1/3 down on the outside. The
bottom 2/3
outside of the mug is MC6G Clear Liner. The XWJ crazed on the inside!
If
anyone is familiar with this glaze can you tell me what happened and how
to fix
it?

Dawn in Tennessee

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

---
Incoming mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.769 / Virus Database: 516 - Release Date: 9/24/2004


---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.769 / Virus Database: 516 - Release Date: 9/24/2004

Ron Roy on fri 1 oct 04


Hi Dawn,

Send me the recipe (XWJ) and I will see if it can be fixed.

RR

>I have used this glaze (from CM) periodically with no problems but I just
>fired a mug with XWJ on the inside and 1/3 down on the outside. The bottom 2/3
>outside of the mug is MC6G Clear Liner. The XWJ crazed on the inside! If
>anyone is familiar with this glaze can you tell me what happened and how to fix
>it?
>
>Dawn in Tennessee

Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
Phone: 613-475-9544
Fax: 613-475-3513