Mary Crabtree on thu 14 oct 04
I've been using Laguna's B-Mix clay for a long time, but my local supplier
has closed and it is getting too difficult for me to get B-Mix anymore.
Any suggestions on a substitute, and who supplies it?
Thanks
Mary
Cynthia Bracker on thu 14 oct 04
Where are you geographically?
Mary Crabtree wrote:
>I've been using Laguna's B-Mix clay for a long time, but my local supplier
>has closed and it is getting too difficult for me to get B-Mix anymore.
>Any suggestions on a substitute, and who supplies it?
>
>Thanks
>Mary
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>
>
>
>
claybair on thu 14 oct 04
Mary,
Where are you located?
Many local suppliers make
a similar clay body.
Gayle Bair
Bainbridge Island, WA
http://claybair.com
-----Original Message-----
From: Mary Crabtree
I've been using Laguna's B-Mix clay for a long time, but my local supplier
has closed and it is getting too difficult for me to get B-Mix anymore.
Any suggestions on a substitute, and who supplies it?
Thanks
Mary
| |
|