Have you got John & Ron's book Mastering Glazes, Cone 6?
They have a wide assortment of Blues in the book and the base glazes are =
great, and fun to play with to alter colours.=20
The colour you want would be relatively easy I should think - just =
modify the amount of cobalt and copper in the Hi Calcium semi matte base =
1 or the glossy base 2. You will probably want to reduce the rutile as =
well since I'll bet your client doesn't want too interesting a Royal =
Blue.