Hello all-

I have been using Waterfall brown for a year or so, and have noticed degredation of quality over time. Made new 10,000 batch and it wasn't the same at all! suspect rutile changes. However, made a very small 500g test batch to see if i didn't screw up the remixing through distraction or just plain duh!, and the test batch was perfect! just what it was supposed to be. Duh!
So, will rescreen current batch, and make 2000 g batch to test larger amount before getting carried away again.

gregg

where it is raining and snowing like crazy!! would love, just love, to go skiing, but too many pots to make for xmas.


Gregg Allen Lindsley
Earth and Fire Pottery
Instructor - Mendocino College
Board Member Potters Council
Mail only: PO Box 402
Cobb, Ca. 95426
UPS etc.: 10325 Brookside Drive
Whispering Pines, Ca. 95426
e mail: gerrg@yahoo.com
http://www.earthandfirepottery.net

---------------------------------
Do you Yahoo!?
Yahoo! Mail Address AutoComplete - You start. We finish.