Allyson May on wed 27 oct 04


Hey Ben,
I have been following the thread with your problems with blue on black. =
I have just finished firing a couple of loads in which I used Licorice =
(M^6G) on tumblers with a dip of Variegated Blue (M^6G) at the rim. =
These are stunning! I also did a few coffee mugs the same way and they =
are also winners. Makes me wish I had glazed them all this way! I use =
Laguna ^6 porcelain and a Laguna ^6 white stoneware and the results are =
pretty much identical. I keep the Licorice pretty thin because I have =
heard others say they have experience running with this glaze. I myself =
have never had a problem of any kind with this glaze. Hope this helps. =
Good luck with your search.
Peace,
Allyson May