Allyson=2E

I've used licorice/rr black for years=2E=2E=2Emy most consistent/dependabl=
e glaze=2E
I also get the teadust effect pretty regularly=2E I haven't narrowed down=

the cause=2E=2E=2Ethink it's the slow cooling=2E I prefer it without the =
teadust=20
myself=2E
I too would be interested in the chemical comp that's creating it=2E Soun=
ds
like an good glaze research project=2Ehmmmmmm=2E=2E