Hi, I have had about 10 glaze firings in my fibre lined LPG kiln and =
still have a great deal of trouble
with consistent results. Sometimes it reduces beautifully, other times =
not at all and others only partial reduction. It is driving me crazy !! =
I seem to have tried all known combinations of blocking off primary =
air/damper etc. Has anyone else had these problems ? How did you solve =
it ?
I am planning another glaze firing this sunday - any advice would be =
truly welcome.

Look forward to your advice.