Ben Friesen on sat 13 nov 04
Hi again,=20
Another problem. I tried your suggestion, Ron, of replacing my black and =
blue combo with your Licorice and the Blue (Light Stormy Blue) over =
dipped. My first test pot came out not too bad... the blue was too dark =
but it seemed like maybe I had something. Now in another load another =
test pot of the same glaze combo just simply pulled away everywhere and =
ran off the pot leaving large areas of raw ware from top to bottom.=20
It seems like this problem is suddenly affecting me on various glazes... =
I must be doing something really wrong.... :(=20
Once again, any ideas? Thank-you kindly,
Ben Friesen
Stonepath Pottery