Louis Katz on sat 13 nov 04


Funny how my toner fires cobalt blue (just like cobalt) at cone ten and
fires a cobalt purple at 1500 degrees F.

ABout rubber gloves, I would read the toner's MSDS and warning labels
on the package first and decide about gloves second

I never believe anything an academic says.

Professor Louis Katz

On Nov 13, 2004, at 10:16 AM, Ditmar wrote:

> Don't go wearing your rubber gloves and mask yet ! There is NO cobalt
> or nickel in photocopy toner.
> There is no economic sense for a manufacturer to use it. It's
> expensive and a potential liability.
> A very technical but thorough paper is at this link for anyone
> interested.
>
>
> http://www.chem.sc.edu/faculty/morgan/pubs/
> EganGalipoKochanowskiMorgan_AnalBioanalChem2003.pdf
>
>
> Toner is primarily an opaque black......iron oxide or lampblack, with
> a plastic carrier that fuses it all to the paper when heated.
>
> Ditmar
>
> _______________________________________________________________________
> _______
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
>
Louis Katz
http://www.tamucc.edu/~lkatz

Ditmar on sat 13 nov 04


Don't go wearing your rubber gloves and mask yet ! There is NO cobalt =
or nickel in photocopy toner. =20
There is no economic sense for a manufacturer to use it. It's expensive =
and a potential liability.
A very technical but thorough paper is at this link for anyone =
interested.

=
http://www.chem.sc.edu/faculty/morgan/pubs/EganGalipoKochanowskiMorgan_An=
alBioanalChem2003.pdf


Toner is primarily an opaque black......iron oxide or lampblack, with a =
plastic carrier that fuses it all to the paper when heated.

Ditmar