Marcia Selsor on tue 16 nov 04
I use three small tanks in tandem with one or two burners. I can fire
when its pretty cold. I get the best color then.
The three tanks togther are slow to freeze up. I can fire for several
hours on 2.5 to 3 pounds pressure and get several firing after the
initial 45 minute start up. The following firings are faster, 30
minutes.
Marcia Selsor
back from North Carolina where I went swimming with porpoises on NOV 5!
| |
|