search  current discussion  categories  kilns & firing - cones & controllers 

we don't need no stinkin' oxyprobe . link to cm article on sniffer.

updated wed 17 nov 04

 

Angela Davis on tue 16 nov 04


Wayne,
I just received John Britt's new book and am all "fired up".
When I got to the oxy probe page I went looking online for more info.
I found this link from CM you might be interested in.

http://www.ceramicsmonthly.org/mustreads/sniffer.asp

Angela Davis

All I can tell you is that if you haven't bought the book yet you
need to go get it. Wonderful pots and a full course on high-fire glazes.



----- Original Message -----
From:
To:
Sent: Tuesday, November 16, 2004 4:59 AM
Subject: Re: We don't need no stinkin' oxyprobe but we can have one!


outflow (far) end. The pipe should be cool enough at that point not
to destroy the sensor or fan. Hmmmmm...time for more engineering.

clink.com.