search  current discussion  categories  glazes - cone 4-7 

cone 6 soda

updated wed 8 dec 04

 

Mark Knott on wed 24 nov 04


i'm wondering if there are other people on the list doing c/6 soda firings? i would be most interested in sharing glazes and or results. i am new to this temp. and do not have a full compliment of glazes. hope to hear from all in this area. thanks, mark knott

Grace Sheese on mon 29 nov 04


Mark,
Check out Julia Galloway's website. All of her work is soda fired to =
cone 6. She shares some of her glazes on her site. =
www.juliagalloway.com

Best of luck,
Grace
www.gracesheese.com

Mark Knott on mon 29 nov 04


grace, thanks for the thought. i do have julia's glazes and have had some good luck with some of them. i was hoping to add to the pallet. just fired another kiln and hope to get some new glazes out of the test i've done. by the way your work is so beautiful. i especially love the stacking jars. very cool. thanks mark knott. www.americanpotters.com key word mark knott
>
> From: Grace Sheese
> Date: 2004/11/29 Mon PM 06:25:48 EST
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: cone 6 soda
>
> Mark,
> Check out Julia Galloway's website. All of her work is soda fired to cone 6. She shares some of her glazes on her site. www.juliagalloway.com
>
> Best of luck,
> Grace
> www.gracesheese.com
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>

Mark Knott on tue 7 dec 04


grace, thanks for the thought. i do have julia's glazes and have had some good luck with some of them. i was hoping to add to the pallet. just fired another kiln and hope to get some new glazes out of the test i've done. by the way your work is so beautiful. i especially love the stacking jars. very cool. thanks mark knott. www.americanpotters.com key word mark knott
>
> From: Grace Sheese
> Date: 2004/11/29 Mon PM 06:25:48 EST
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: cone 6 soda
>
> Mark,
> Check out Julia Galloway's website. All of her work is soda fired to cone 6. She shares some of her glazes on her site. www.juliagalloway.com
>
> Best of luck,
> Grace
> www.gracesheese.com
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>