search  current discussion  categories  glazes - cone 04-06 

date: tue, 30 nov 2004 20:54:38 -0600from: kevin komadina

updated fri 3 dec 04

 

Rogier Donker on thu 2 dec 04

Subject: L & L Kiln

Err1 is ALWAYS! supply! Your light load fired OK because it did not take a
lot of juice to get up to temp. When you loaded the kiln with lots of tiles,
you increased the need for juice in order to get hot enough....the computer
was pulling all the juice it could, but finally had to shut down as there
was not enough juice available for the need...Check the voltage on the kiln
name plate, then check the supply....More than likely your kiln is 220-240V
but you only have 208 or even less available...:-(
Rogier Donker
http://www.donkerstudio.org