> > On Tue, 30 Nov 2004 09:40:28 -0800, Rikki Gill
wrote:
>
> > >Hi Maura,
> > >Here it is. Good luck
> > >
> > >Troy slip
> > >
> > >albany 150
> > >rutile 20
> > >R.I.O. 20
> > >feldspar 10
> > >
> > >I used custer
> > >
> > >Rikki Gill
> >
> >
> >
> > What cone is this slip?
>
> 10-11
>
> Is it vitreous at the proper cone?
probably
>
> Do you use
> > the slip under glazes?
>
> no
>
> If so, how does it react?
>
> I don't know. It is fine on glazes
>
> Thanks for sharing your
> > recipe.
> >
> you are welcome.
Maura on sun 5 dec 04
Ah Rikki,
You didn't forget! Thanks so very much. Just scanning the discussions and
saw that you'd sent the recipe. Yipee! There are so many people waiting to
share it. It amazes me how the web can connect us.
Thanks for your kindness,
Maura
| |
|