search  current discussion  categories  glazes - cone 4-7 

cranberry slip for cone 6? commercial glaze works well

updated thu 9 dec 04

 

Kathy McDonald on wed 8 dec 04


I have used Mayco Stroke and Coat glazes quite successfully for this
technique.
They seem to have enough clay content that you can use them as they come out
of the bottle,
and I have also mixed them with a bit of B mix slurry and they work really
well for me.

Saves all the time guessing about color concentration and the range of
colors are wonderful.

The Reds also do well right to cone 10, Salsa and Cherry Bomb are my
favorites.

Kathy
(Who has no affiliation with Mayco, but thinks that particular product is
great)
---