John Norris on sat 11 dec 04


Folks-

A while back I made pinhole cameras with ceramic bodies. The majority of=

the camera was out of clay, but the pin hole and shutter were from copper=
.

I used paper negatives and was able to come up with some pretty good imag=
es.
The cameras themselves looked quite good. (If I do say so myself.) I'l=
l
need to scan and get a few pictures of them up on my website. Almost had=

them published in the Pinhole Journal...

If you are curious about these, you can pretty easily get images and usin=
g
paper negatives is a cheap way to go.

Here's the place to start-

http://www.pinholeresource.com/

John