search  current discussion  categories  materials - plaster 

plaster problem/mixing,etc.--ideal studio

updated fri 31 dec 04

 

Jim Kasper on thu 30 dec 04


I want to second that. I picked up a copy when I visited the
ACC. Besides being a great general read, when I occasionally mix
plaster, I pull it out to check the numbers. It also came in handy
when mixing coloered slips.
Regards,
Jim
http://zafka.com

--- In clayart@yahoogroups.com, Vince Pitelka wrote:
> Please forgive me for what will seem like merciless plug of my
book, but,
> my book "Clay: A Studio Handbook" contains the plaster mixing tables
> provided by US Gypsum, manufacturers of most of the plaster products
we use
> in the studio. It really makes things simple.
> Best wishes -
> - Vince