Edouard Bastarache Inc. on fri 7 jan 05
Hello Ivor,
I forgot to tell you that after having lowered the alumina=20
portion down to .300, I also lowered the silica portion to
3.0 with good results. The base recipe became :
Custer spar 59
Whiting 22
Silica 19
Later,