Nancy Udell on wed 12 jan 05


Hi Cherie, Depending on what kind of slip you are using, you can just
wait for the water to settle on top and then pour some off.
This may be too simple an answer, but hey, what the heck.

Nancy in Md, looking forward very much to NCECA.

Date: Tue, 11 Jan 2005 01:41:28 -0500
From: Cherie W
Subject: Thicken Slip?

Hi, is it possible to thicken slip? Can I add something to it to make
it a thicker consistancy?? Thank You Cherie

-----------------------------