In recipes for repair of bisque in the archives there are references to
using sodium silicate and various clays.
Can anyone tell me what sodium silicate might be called here in Mexico and
what might be a substitute. Gracias.

william schran on sun 16 jan 05


Fran wrote:> Can anyone tell me what sodium silicate might be called
here in Mexico and
what might be a substitute.<

It's also called water glass or egg keep.
Bill

pdp1@EARTHLINK.NET on sun 16 jan 05


Hello,


(You should consider to sign your posts so responses to them
may enjoy salutations! senders e-mail address or appearent
names in them only sometimes are those of the actual
sender...)

Somehow your question interested me...so...here are some
things which maybe could contribute to the resolution...


Sodium = s. sodio; adj. sódico; de sodio

Silicate = s. silicato



This might help also, as for provideintg more industry and
manufactureing names and terms -

Chemical Name: Silicic acid, sodium salt
CAS No: 1344-09-8
Synonyms: Silicic acid, sodium salt;49FG;Agrosil LR;Agrosil
S;AS BOND 1001;Britesil;Britesil H 20;Britesil H
24;CARSIL;Carsil (silicate);Caswell No. 792;Chemsilate;DP
222;DRYSEQ;DUPONT 26;EPA Pesticide Chemical Code 072603;GM
10 (silicate);HK 30 (VAN);L 96 (SALT);METSO 99;N 38;N 38
(silicate);Portil A;PYRAMID 1;PYRAMID 8;Q 70;Ru
Silicate;SIKALON;SILICA E;SILICA K;SILICA N;SILICA
R;Silican;SILICIC ACID, SODIUM SALT;SODIUM
BETA-SILICATE;SODIUM SESQUISILICATE;Sodium silicate;Sodium
silicate glass;Sodium silicate solution;SODIUM
SILICONATE;SODIUM WATER GLASS;Soluble glass;Star;waterglass



Chemical Name: Silicic acid, sodium salt
CAS No: 1344-09-8
Synonyms: Silicic acid, sodium salt;49FG;Agrosil LR;Agrosil
S;AS BOND 1001;Britesil;Britesil H 20;Britesil H
24;CARSIL;Carsil (silicate);Caswell No. 792;Chemsilate;DP
222;DRYSEQ;DUPONT 26;EPA Pesticide Chemical Code 072603;GM
10 (silicate);HK 30 (VAN);L 96 (SALT);METSO 99;N 38;N 38
(silicate);Portil A;PYRAMID 1;PYRAMID 8;Q 70;Ru
Silicate;SIKALON;SILICA E;SILICA K;SILICA N;SILICA
R;Silican;SILICIC ACID, SODIUM SALT;SODIUM
BETA-SILICATE;SODIUM SESQUISILICATE;sodium silicate;sodium
silicate glass;sodium silicate solution;SODIUM
SILICONATE;SODIUM WATER GLASS;Soluble glass;Star;Waterglass

Chemical Name: Silicic acid (H2SiO3), disodium salt
CAS No: 6834-92-0
Synonyms: Anhydrous sodium
metasilicate;B-W;CRYSTAMET;Disodium metasilicate;Disodium
monosilicate;Metso 20;Metso beads 2048;METSO BEADS,
DRYMET;Metso pentabead 20;ORTHOSIL;Silicate de
Sodium;Silicic acid (H2SiO3), disodium salt;Silicic acid,
disodium salt;SIMET A;Sodium metasilicate;SODIUM
METASILICATE (NA2SIO3);Sodium metasilicate, anhydrous;sodium
silicate;sodium silicate (NA2SIO3);Soluble glass;WATER GLASS


Too, you could try going on 'Amazon.com' and looking for
these Books under 'used books', otherwise, these are a bite
in the ass to buy new...


Wiley's English-Spanish Spanish-English Chemistry Dictionary
Steven M. Kaplan
ISBN: 0-471-24923-8
Paperback
544 pages
February 1998

Wiley's English-Spanish Spanish-English Chemistry Dictionary
Steven M. Kaplan
ISBN: 0-471-19288-0
Hardcover
530 pages
February 1998

English-Spanish, Spanish-English
Chemistry Dictionary
by Steven M. Kaplan


Good luck,

Phil
le ve


----- Original Message -----
From: "Fran Schwartz"


> In recipes for repair of bisque in the archives there are
references to
> using sodium silicate and various clays.
> Can anyone tell me what sodium silicate might be called
here in Mexico and
> what might be a substitute. Gracias.