search  current discussion  categories  glazes - specific colors 

black-in-black-effect

updated sat 29 jan 05

 

Petra Hahn on fri 28 jan 05


Hi all,
thanks for your suggestions. But I already knew that the "normal" techniq=
ue
is to smoke the pieces.
My aim is to make functional pots in a stoneware firing between 1200=B0 a=
nd
1260=B0.
And I don't think that high fired pots take up the smoke if I do it
afterwards. Or does that work?
I'm going to make some attempts with an almost black clay and thin spraye=
d
transparent glaze.

have a nice weekend
Petra