search  current discussion  categories  glazes - misc 

a+ for hyperglaze

updated thu 10 feb 05

 

Steve Slatin on tue 8 feb 05


Sam --

I've never used Hyperglaze so can't compare, but
GlazeMaster does have functions to calculate triaxial,
line, Currie Grids and quadraxial blends.

The print function you mention is one I've never
gotten from GlazeMaster (but then again I've never
tried -- I do see how it's advantageous to reduce
paper waste, but I often use bits of paper for various
things in the studio so I'm kind of careless about
conservation in that area). It does sound useful.

Best wishes -- Steve Slatin

--- Sam Hoffman wrote:

> Hi Lou-
>
> I give Hyperglaze 2 out of 2 thumbs up; I
> simply love this software.
> I've been using it for over 6 years, and find it to
> be much better than
> all of the competing programs, including Insight and
> GlazeMaster.
> (sorry, John...) It does all of the normal data
> base/storage functions
> with ease and elegance, but also has powerful
> triaxial and quadraxial


=====
Steve Slatin -- Don't Ever Antagonize The Horn

__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

Sam Hoffman on tue 8 feb 05


Hi Lou-

I give Hyperglaze 2 out of 2 thumbs up; I simply love this software.
I've been using it for over 6 years, and find it to be much better than
all of the competing programs, including Insight and GlazeMaster.
(sorry, John...) It does all of the normal data base/storage functions
with ease and elegance, but also has powerful triaxial and quadraxial
blend components. Included in the software is a well written
explanation of Unity Theory and detailed information about glaze
formulation.
What I like best about Hyperglaze is the ability to print a single
glaze or groups of glazes in several different ways. In the OS9
version, one could print up to 6 recipes on 1 page, which was ideal for
making lots of tests while conserving paper. I am actually having
trouble with the first OSX version getting this feature to work, but
hopefully Richard Burkett is addressing that with the first upgrade.
The $100 pricetag is a little bit staggering, but is par for course
these days. I'm willing to bet there is a 30 guarantee on the
software, so I'd recommend giving it a whirl. Let me know if you have
any questions about specific features...

-Sam


S.L. Hoffman Pottery
Corvallis, Oregon
www.samhoffman.com


On Feb 7, 2005, at 10:13 AM, Lou Roess wrote:

> Hi, having checked the archives and read as much as I can absorb , I'm
> wondering if someone who uses Hyperglaze software with MacOSX can tell
> me more about it before I fork over $100. My interest is not so much
> in formulating new glazes as in determining if the ones I'm using or
> contemplating using are within acceptable limits for my cone 6 electric
> firings and tweaking them if they're not.
> Any help would be greatly appreciated
> TIA
> Lou in Colorado.
>
> _______________________________________________________________________
> _______
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>