kiln shelf grumble- thanks

updated wed 9 feb 05

 

barblund on tue 8 feb 05


Hi folks, thanks for the input. I am not going to go into the glaze =
problem- its one I am fiddling with right now. I will try Tony's wash =
recipe and hope it helps. It is important that I can scrape all of the =
wash off the shelf from time to time without destroying my elbow joints =
so that I can turn the shelves over to straighten out the inevitable =
warping.

Is anyone using the ceramic paper on their shelves at this time?

Barb in Bloomington