Alisa Liskin Clausen on thu 10 feb 05
On Wed, 9 Feb 2005 17:38:09 -0600, Lori Doty wrote:
>I love the colors of the EC frosty white with cobalt WOW electric blue.
>Did you fire that on porcelain or is that stone ware?
>
>Any way just love it.
>
>
Dear Lori,
My clay is either a white mid range stoneware or the same with iron specs.
both with 20% 0-2cm. grogg.
The glaze is elelctric blue, but as you can see, it runs like the devil.
Both of the glaze tests with Cobalt and Copper ran down to the kiln shelf.
I put prefired slabs about 4 inches thick in various lengths under all of
the tests. Glad I do.
regards from Alisa in Denmark
| |
|