search  current discussion  categories  glazes - specific colors 

alisa/ purple opal glaze adding up to 89

updated wed 16 feb 05

 

Alisa Clausen on wed 16 feb 05


> HI Alisa,
> I'm wondering if you left something out of this recipe. The glaze
> ingredients only total 89. Is there something omitted?
>
> John Post
> ------------------------------------------------------------------------
> ----------------------------
>
>
> Glaze test for Purple Opal, cone 6 ox.
> Recipe:
> 14 Gerstely Borate
> 30 Spodumene
> 5 EPK
> 7 Dolomite
> 13 Talc
> 20 Silica
>
>
> ADD
> 6 Rutile
> 1 Manganese Diox.
> Underlying glaze is a mat tan. Over the mat tan ground is a streaky
> white and opalescent gloss shell. Overall, the glaze is tan with
> white, feathery streaking.
> or
> 2 Cobalt Carb.
> A dark blue purple mat glaze.
> or
> 4-6 Copper Carb.
> A semi mat glass green glaze.
>






Dear John,
I could not get Clayart's server to answer you. Unfortunately, fortunately,
nothing is left out. As you know recipes, do not have to add up to 100, it
is just convenient for the math. However, this is a recipe I have tried
under different names, and could not believe that I got duped again! It has
never produced anything else but beige and streaky in my firings, but maybe
something else for you. It is also called POP.

thanks for writing, regards from Alisa in Denmark
very excited to open the tests tomorrow of lichens, crawls and Gartsides.