search  current discussion  categories  materials - frits 

glaze test correction kemp glaze uses frit 3134 not 3124.

updated tue 22 feb 05

 

Alisa Clausen on mon 21 feb 05


Bacia rightfully pointed out, that I listed=20
Brian Kemp Lichen Glaze
with Frit 3124.

It should read Frit 3134.

I used my local Boron Frit and it
worked very well.

regards from Alisa