standard for microwave use of ceramic/glass under development

updated wed 23 feb 05

 

Daniel Semler on tue 22 feb 05


Hi All,

For those who are interested in the issue of microwave safe functional ware, I
was just checking out some standards on the ASTM website. It appears that they
are working on a standard test method for microwave safety of glass and
ceramics for reheating. Reheating is defined as being less than 5 mins. After
that its cooking, according to WK4454, but hey its a start.

For reference the title and number is, WK4454 Standard Test Method for
Determination of Microwave Safe for Reheating for Ceramic and Glassware.
Here's a URL
http://www.astm.org/cgi-bin/SoftCart.exe/DATABASE.CART/WORKITEMS/WK4454.htm?L+mystore+pzzj6324+1109069762
No idea when it might be published.

Thanx
D

----------------------------------------------------------------