wood firing to c.6

updated fri 25 feb 05

 

Lili Krakowski on thu 24 feb 05


Yes it has been done. By me inter al. Somewhere I have an article =
about someone who did it. Works perfectly well. Of course certain =
higher fired effects do not happen, but a lot of lower temp ones do. =
Good luck with the project.
Lili Krakowski

Be of good courage