I was going through some files this afternoon and came across some old cone 8 oxidation glazes.
I've put the recipes online if anyone is interested in trying them out. These are glazes that I used
in the 1960s and there are a few nice ones in the group. I'm offering them "as is" since it's been so
long since I used them and can't remember how many of them looked. Try some tests and see
what you think. Here are the recipes:
http://www.steveirvine.com/cone8ox.html

From a still very snowy Big Bay, Ontario,

Steve Irvine
http://www.steveirvine.com

Ken Chin-Purcell on sat 5 mar 05


Thanks Steve. I will post test tiles pictures to Clayart of any that I test.

-- Ken Chin-Purcell
www.bungalowpottery.com


On Sat, 5 Mar 2005 16:52:53 -0500, Steve Irvine wrote:
> I was going through some files this afternoon and came across some old cone 8 oxidation glazes.
> I've put the recipes online if anyone is interested in trying them out. These are glazes that I used
> in the 1960s and there are a few nice ones in the group. I'm offering them "as is" since it's been so
> long since I used them and can't remember how many of them looked. Try some tests and see
> what you think. Here are the recipes:
> http://www.steveirvine.com/cone8ox.html
>
> From a still very snowy Big Bay, Ontario,
>
> Steve Irvine
> http://www.steveirvine.com
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>