search  current discussion  categories  kilns & firing - coatings 

itc 213 salt

updated tue 8 mar 05

 

tim storey on mon 7 mar 05


This is my 30th year salt firing and I've chewed up a lot of burner tips
getting here. I received a free sample of itc213 for praising itc100 on a
forge building Blacksmith] website, I coated the used burner tip and all
exposed metal on my wife's forge with itc213 and 4 years of daily operation
they look like new! I put some on my admittedly old and tatty venturi burner
tips [heritage burners /plainsman] and after 30 cycles [cone 10] they have
not deteriorated to the extent I would expect, I also salt through the burner
ports so this is an exreme test When I put new tips on I will for certain
use it again.